Sn42/Bi58

LOW TEMPERATURE ALLOY

Sn42/Bi58

LOW TEMPERATURE ALLOY

Sn42/Bi58

LOW TEMPERATURE ALLOY

Sn42/Bi58 Low Temperature Alloy

Sn42/Bi58 is a low melting temperature alloy composed of 42% tin, 58% bismuth. Low temperature solders require a lower peak reflow temperature than other lead-free solder alloys reducing energy consumption and component-warpage related defects such as NWO (non-wet opens).

Sn42/Bi58 alloy is available with specially formulated fluxes to ensure solder joint integrity and high electrochemical performance, even at reduced reflow temperatures.

Features

✔ Manufactured with AIM Electropure™ Technology
✔ Good Fatigue Characteristics
✔ Improved Wetting
✔ Low Temp Alloy: Melting Point:138°C
✔ RoHS Compliant
✔ Complies with IPC J-STD-006

Application Use

✔ Lead-free low melt alloy
✔ Low temperature solder paste reduces overall reflow profile temperature significantly lower than SAC305 (217-219℃)
✔ Reduces NOW/HiP defects on temperature sensitive components
✔ Good wetting performance required for quick, post-assembly attachments

Technical Features of Sn42/Bi58
Composition Melting Temperatures (℃) Peak Reflow Temperature (℃) Cost Level
Sn/Bi/Ag 138°C 235°C $$
Product TDS of Sn42/Bi58 Low Temperature Alloy

Download the Sn42/Bi58 product TDS of to learn more about its key features, technical structure, and application areas.

Similar Products